Introduction to the metallurgical principles which have guided the development of the superalloys, for senior undergraduate and postgraduate students.
Introduction to the metallurgical principles which have guided the development of the superalloys, for senior undergraduate and postgraduate students.
Über den Autor
Roger C. Reed is Professor and Chair in Materials Science and Engineering at Imperial College London. He is widely known for his work on the physical metallurgy of the superalloys.
Inhaltsverzeichnis
1. Introduction; 2. The physical metallurgy of nickel and its alloys; 3. Single crystal superalloys for blade applications; 4. Superalloys for turbine disc applications; 5. Environmental degradation: the role of coatings; 6. Summary and future trends.
Details
Erscheinungsjahr: | 2008 |
---|---|
Fachbereich: | Chemische Technik |
Genre: | Importe, Technik |
Rubrik: | Naturwissenschaften & Technik |
Medium: | Taschenbuch |
ISBN-13: | 9780521070119 |
ISBN-10: | 0521070112 |
Sprache: | Englisch |
Einband: | Kartoniert / Broschiert |
Autor: |
Reed, Roger C.
Roger C., Reed |
Hersteller: | Cambridge University Press |
Verantwortliche Person für die EU: | Libri GmbH, Europaallee 1, D-36244 Bad Hersfeld, gpsr@libri.de |
Maße: | 244 x 170 x 22 mm |
Von/Mit: | Roger C. Reed (u. a.) |
Erscheinungsdatum: | 15.04.2008 |
Gewicht: | 0,675 kg |
Über den Autor
Roger C. Reed is Professor and Chair in Materials Science and Engineering at Imperial College London. He is widely known for his work on the physical metallurgy of the superalloys.
Inhaltsverzeichnis
1. Introduction; 2. The physical metallurgy of nickel and its alloys; 3. Single crystal superalloys for blade applications; 4. Superalloys for turbine disc applications; 5. Environmental degradation: the role of coatings; 6. Summary and future trends.
Details
Erscheinungsjahr: | 2008 |
---|---|
Fachbereich: | Chemische Technik |
Genre: | Importe, Technik |
Rubrik: | Naturwissenschaften & Technik |
Medium: | Taschenbuch |
ISBN-13: | 9780521070119 |
ISBN-10: | 0521070112 |
Sprache: | Englisch |
Einband: | Kartoniert / Broschiert |
Autor: |
Reed, Roger C.
Roger C., Reed |
Hersteller: | Cambridge University Press |
Verantwortliche Person für die EU: | Libri GmbH, Europaallee 1, D-36244 Bad Hersfeld, gpsr@libri.de |
Maße: | 244 x 170 x 22 mm |
Von/Mit: | Roger C. Reed (u. a.) |
Erscheinungsdatum: | 15.04.2008 |
Gewicht: | 0,675 kg |
Sicherheitshinweis